NOTE The determination of these parameters can be relevant for thermal insulating products intended for application to stainless austenitic steel surfaces. The presence of chloride, fluoride, silicate and sodium ions under certain conditions can influence the risk of stress corrosion cracking. See Annex B for further information on general use of this document.
ENISO 12624