1.1 This test method defines conditions for the use of differential scanning calorimetry (DSC) with fluoropolymers. It covers the use of DSC analyses with the fluoropolymers, PTFE, PVDF, PCTFE, and PVF and their copolymers PFA, MFA, FEP, ECTFE, EFEP, VDF/HFP, VDF/TFE/HFP, VDF/ CTFE. The test method is applicable to the analysis of powders as well as samples taken
from semi-finished or finished products. The nature of fluoropolymers is such that
special procedures are needed for running DSC analysis and interpreting the results.