This document specifies requirements for qualification testing of welding procedure specifications (WPSs) for electron or laser beam welding.
This document applies to metallic materials, irrespective of the shape of the parts, their thicknesses, the manufacturing method (e.g. rolling, forging, casting, sintering) or their heat treatment. It covers both the production of new parts and repair work.
ISO 15614-11:2025
EN ISO 15614-11:2025