ISO 15609 series covers the specification and qualification of welding procedures for metallic materials.
ISO 15609‑2 is the second part in the multi-series of documents that specifies requirements for the content of welding procedure specifications for gas welding processes. The main objective of ISO 15609‑2 is to improve quality assurance systems in the field of welding.
ISO 15609-2 on gas welding procedures for metallic materials is applicable to:
ISO 15609‑2 specifies requirements for the content of welding procedure specifications for gas welding processes. The variables listed are those which influence the quality of the welded joint.
ISO 15609‑2 helps you standardize the specification and qualification for the content of welding procedure specifications for gas welding processes. Having a common point of reference for classification improves the efficiency of gas welding processes across the welding industry.
Organizations should use ISO 15609‑2 for help with the design, materials and condition of their gas welds. As a result, you can enhance quality assurance and quality management systems in the field of welding. This can ultimately help build trust and gain acceptance across the welding industry and supply chain.
BS EN ISO 15609-2:2019 supersedes BS EN ISO 15609-2:2001, which is withdrawn. BS EN ISO 15609-2:2019 includes some technical changes with respect to BS EN ISO 15609-2:2001. These include:
EN ISO 15609-2
ISO 15609-2