Requirements for the content of welding procedure specifications for arc welding processes.
This International Standard specifies requirements for the content of welding procedure specifications for arc welding processes.
This standard is part of a series of standards; details of this series are given in the annex to EN ISO 15607:2003.
The variables listed in this standard are those influencing the quality of the welded joint.
This International Standard supersedes BS EN 288-2:1992 which is withdrawn.
It includes the following cross references:
EN 439, EN 26848, EN ISO 4063, EN ISO 6947, CR ISO 15608.
ISO 15609-1:2004
ISO 15609-1:2004/Cor 1:2005