Search BSI Knowledge
Cookie Settings
ISO 14322:2012 | 15 Jun 2012 | BSI Knowledge
Standard
Withdrawn
Shop Exclusive
ISO 14322:2012
Plastics. Epoxy resins. Determination of degree of crosslinking of crosslinked epoxy resins by differential scanning calorimetry
Published:
15 Jun 2012
•
Withdrawn:
19 Jul 2018
Overview
Preview
References
History
Visit the preview section for more information
Product Details
Descriptors
—
ICS Codes
83.080.10 Thermosetting materials
Committee
PRI/42
International relationships
—
ISBN
—
Publisher
ISO