Search BSI Knowledge
Cookie Settings
BS EN ISO 11357-1:1997 | 15 Jul 1997 | BSI Knowledge
Standard
Withdrawn
BS EN ISO 11357-1:1997
Plastics. Differential scanning calorimetry (DSC) - General principles
Published:
15 Jul 1997
•
Withdrawn:
30 Nov 2009
Overview
Preview
References
History
Visit the preview section for more information
Product Details
Descriptors
Differential thermal analysis
Test equipment
Temperature
Thermal analysis
Melting point
Moulded materials
Testing conditions
Thermosetting polymers
Thermodynamic properties
Calibration
Composite materials
Plastics
Scanners
Definitions
Thermoplastic polymers
Test specimens
Heat measurement
ICS Codes
83.080.01 Plastics in general
Committee
PRI/21
International relationships
Identical to:
ISO 11357-1:1997
ISBN
0 580 27579 5
Publisher
BSI