Search BSI Knowledge
Cookie Settings
BS EN ISO 11357-4:2014 | 31 Jul 2014 | BSI Knowledge
Standard
Withdrawn
BS EN ISO 11357-4:2014
Plastics. Differential scanning calorimetry (DSC) - Determination of specific heat capacity
Published:
31 Jul 2014
•
Withdrawn:
2 Mar 2021
Overview
Preview
References
History
1 Scope
This part of ISO 11357 specifies methods for determining the specific heat capacity of plastics by differential scanning calorimetry.
Product Details
Descriptors
Plastics and rubber technology
Thermal measurement
Thermal analysis
Specific heat
Plastics
Heat measurement
Quantitative analysis
Differential thermal analysis
Scanners
ICS Codes
83.080.01 Plastics in general
Committee
PRI/21
International relationships
Identical to:
EN ISO 11357-4:2014
ISO 11357-4:2014
ISBN
978 0 580 84698 4
Publisher
BSI