1 Scope
This part of ISO 11357 specifies methods for the determination of oxidation induction
time (isothermal OIT) and oxidation induction temperature (dynamic OIT) of polymeric
materials by means of differential scanning calorimetry (DSC). It is applicable to
polyolefin resins that are in a fully stabilized or compounded form, either as raw
materials or finished products. It may be applicable to other plastics.