BS 3500-3:1969 | 20 Oct 1969 | BSI Knowledge
Standard
Withdrawn
BS 3500-3:1969
Methods for creep and rupture testing of metals - Tensile creep testing
Published:
20 Oct 1969
•
Withdrawn:
15 Dec 2000
Overview
Preview
References
History
Visit the preview section for more information
Product Details
Descriptors
Creep testing
Test specimens
Testing conditions
Dimensions
Design
Tensile testing
Mechanical testing
Test equipment
Metals
ICS Codes
77.040.10 Mechanical testing of metals