1.1 This document specifies the electrochemical test for determining galvanic corrosion
rate of CFRPs and metal assemblies with protection-coating, subjected to the corrosive
environment of electrolyte diffusion through the coating. It specifies the apparatus,
the test solutions, and the procedure to be used in conducting the electrochemical
tests for
-
a) the assessment of the Fick's diffusion parameter for protective coating on metallic
materials, and
-
b) the estimation of the galvanic corrosion rates with the conversion of ISO 21746 coating-free sample data.