ISO 7539‑10 is the 10th part of a multi-series standard. It deals with stress corrosion testing for metals and alloys using the reverse U-bend method.
ISO 7539‑10 specifies procedures for designing, preparing and using reversed U-bend (RUB) test specimens for investigating the susceptibility of the metal to stress corrosion cracking.
ISO 7539‑10 introduces very severe stresses in a high corrosion resistance metal, with minimum relaxation, in order to enhance the likelihood of inducing stress corrosion cracking.
ISO 7539‑10 on stress corrosion testing for metals and alloys is applicable to:
Corrosion in metal equipment or structures can compromise their functionality. Prolonged corrosion on metals can inflict severe stress on them and devaluate the metals physical properties. Regular tests should be performed to identify corrosion stress in metals to keep them well maintained.
ISO 7539‑10 provides you with guidance on the reverse U-bend method for corrosion stress testing. It is used as a screening test for tubing, piping, plate, bar and other products including welded materials. The RUB test is a particularly effective test for assessing susceptibility to stress corrosion cracking.
The RUB test described in ISO 7539‑10 is simple and provides rapid screening of corrosion cracking for metals and alloys
BS EN ISO 7539‑10:2020 supersedes BS EN ISO 7539‑10:2014, which is now withdrawn.
Changes in BS EN ISO 7539‑10:2020 include:
EN ISO 7539-10
ISO 7539-10