24/30482190 DC | 1 Feb 2024 | BSI Knowledge
Standard
24/30482190 DC
BS EN ISO 11357-3 Plastics - Differential scanning calorimetry (DSC) - Part 3: Determination of temperature and enthalpy of melting and crystallization
Current
•
Published:
1 Feb 2024
Overview
Preview
References
History
Visit the preview section for more information
Product Details
Descriptors
Thermal analysis
Testing conditions
Scanners
Plastics
Temperature
Mathematical calculations
Melting
Crystallization
Differential thermal analysis
Heat measurement
Thermodynamic properties
ICS Codes
83.080.01 Plastics in general
Committee
PRI/21
International relationships
Identical to:
ISO 11357-3
ISBN
—
Publisher
BSI