BS EN 12373-19:2001 | 15 Jul 2001 | BSI Knowledge
Standard
Withdrawn
BS EN 12373-19:2001
Aluminium and aluminium alloys. Anodizing - Rating system for the evaluation of pitting corrosion. Grid method
Published:
15 Jul 2001
•
Withdrawn:
31 Mar 2011
Overview
Preview
References
History
Visit the preview section for more information
Product Details
Descriptors
Electrodeposition
Corrosion
Pitting corrosion
Anodizing
Aluminium
Oxides
Performance
Anodic coating
Aluminium alloys
Classification systems
ICS Codes
25.220.20 Surface treatment
77.120.10 Aluminium and aluminium alloys